DSC300C Low temperature differential scanning calorimeter, liquid nitrogen refrigeration, high sensitivity. Used to DSC thermal analysis in plastics and rubber industry, can be glass transition temperature test, phase transition test, melting and enthalpy test, product stability, oxidation induction test, etc
DSC-300C Low Temperature Differential Scanning Calorimeter is designed for the measurement of DSC thermal analysis in plastics and rubber industry, can be glass transition temperature test, phase transition test, melting and enthalpy test, product stability, oxidation induction test, etc. Low temperature differential scanning calorimeter DSC300C, liquid nitrogen refrigeration, high sensitivity.
Test standards:
ISO/TR10837:1991, ASTM D3895-1998, ASTM E 967, ASTM E 968, ASTM E 793, ASTM D 3895, ASTM D 3417, ASTM D 3418, ISO 11357-6
Main features:
1. Brand new furnace structure, better resolution and resolution and better baseline stability
2. Parameters can be set to multi-stage heating, constant temperature, cooling
3. The instrument can adopt two-way control (host control, software control), with friendly interface and easy operation
4. Using imported chips, acquisition circuit shielding and anti-interference processing
5. The sensor adopts hot-melt technology instead of traditional spot welding technology, with higher sensitivity
Advantages:
1. The industrial-grade 7-inch touch screen of the DSC300C differential scanning calorimeter displays rich information.
2. DSC300C differential scanning calorimeter has a new metal furnace structure with better baseline and higher precision.
3. USB communication interface, strong versatility, reliable and uninterrupted communication, supports self-recovery connection function.
4. Automatic switching of two air flow rates, fast switching speed and short stabilization time. At the same time, add a protective gas input.
5. The DSC300C differential scanning calorimeter adopts imported chips with high stability.
Technical datas:
Model | DSC-300C | DSC-300L |
Temperature range | -40~600℃ | -170~600℃ |
Temperature resolution | 0.01°C | 0.001℃ |
Temperature fluctuation | ±0.01℃ | ±0.01℃ |
Heating rate | 0.1~100℃/min | 0.1~100℃/min |
Cooling rate | 0.1~40℃/min | 0.1~40℃/min |
DSC range | 0~±600mW | 0~±600mW |
DSC resolution | 0.01uW | 0.01uW |
DSC sensitivity | 0.001mW | 0.001mW |
Temperature control mode | heating, constant temperature, cooling (automatic program control), constant temperature time can be set by yourself | |
Scanning mode | Heating scan, cooling scan | |
Atmosphere control | gas Two-way automatic switching (instrument automatic switching) | |
Display mode | 24bit color, 7-inch LCD touch screen display | |
Program control | can realize six-stage heating constant temperature control, special parameters can be customized | |
Power supply | AC220V/50Hz or 110V, 60Hz | |
Gas flow | 0-300mL/min | |
Gas pressure | ≤5MPa | |
Data interface | Standard USB interface | |
Parameter calibration | Equipped with standard substances (indium, tin, lead), users can correct the temperature |