Wuhan Bonnin Technology Ltd, Laboratory Instruments Expert in China

Product Description

Application

This DSC-1000 DSC differential scanning calorimeter is designed for the measurement of DSC thermal analysis in plastics and rubber industry, can be glass transition temperature test, phase transition test, melting and enthalpy test, product stability, oxidation induction test, etc. (Tg, Tc, Tm, enthalphy of crystallization, enthalphy of melting & crystallinity in %, OIT, etc).

 

Test standards:

ISO/TR10837:1991, ASTM D3895-1998, ASTM E 967, ASTM E 968, ASTM E 793, ASTM D 3895, ASTM D 3417, ASTM D 3418, ISO 11357-6

Product Name
DSC Differential Scanning Calorimeter, DSC Differential Scanning Calorimetry Analyzer, Differential Scanning Calorimeter
Applications
High polymer material industry; High-molecular polymer industry; University; Educational Institutions; Lab; Research Institute ETC.
Function
Oxidation induction time (OIT); Glass transition (Tg); Melt; Crystal; Thermal Stability; Curing / Crosslinking; Cold Crystal; Phase Transition. ETC…

 

Main feature:

1. Industrial-grade 7-inch touch screen with rich display information.
2. New ceramic furnace body structure, better baseline and higher precision. The heating adopts the indirect conduction method, which has high uniformity and stability, and reduces pulse radiation, which is better than the traditional heating mode.
3. USB communication interface, strong versatility, reliable and uninterrupted communication, supports self-recovery connection function.
4. Automatic switching of two air flow rates, fast switching speed and short stabilization time. At the same time, add a protective gas input.
5. The software is simple and easy to operate.

 

Technical datas:

Model DSC-1000
Temperature range room temperature~1050℃
DSC range 0~±800mW
Heating rate 0.1~100℃/min
Temperature resolution 0.01℃
Temperature fluctuation ±0.01℃
Temperature repeatability ±0.1℃
DSC noise 0.01μW
Atmosphere control Nitrogen, Oxygen (instrument switch automatically)
Display mode 24 bit color, 7-inch LCD touch screen display
Data interface standard USB interface
Parameter standard Equipped with standard material (tin), with one-key calibration function, users can calibrate temperature and enthalpy
Software With temperature multi-point correction function
Gas flow 0-300mL/min (other ranges can be customized)
Gas pressure 0.2MPa
Power supply AC220V/50Hz or AC110V/60Hz

Enquiry For DSC-1000 DSC Differential Scanning Calorimeter